Quality & CIPET testing
Our main profile is tested at CIPET against IS 17953 — the Indian Standard for uPVC window and door profiles. Here are the results, and what each test means for your windows.
| Property (as per Indian Standards) | Requirement | Fenplast result | Tested by |
|---|---|---|---|
| Heat reversion — IS 17953 Annex C | Main profile ≤ 2.0% | 1.79% Pass | CIPET |
| Heat ageing at 150 °C — IS 17953 Annex E | No blisters, cavities, cracks, surface peel-off or delamination | Pass | CIPET |
| Tensile bending, L corner — IS 17953 Annex F | — | 584.0 N | CIPET |
| Compression bending, L corner — IS 17953 Annex F | — | 3147.0 N | CIPET |
| Tensile bending, T corner — IS 17953 Annex F | — | 517.0 N | CIPET |
| Compression bending, T corner — IS 17953 Annex F | — | 2124.0 N | CIPET |
| Charpy impact resistance — IS 13360 Part 5 / Sec 5 | > 65 kJ/m² | 71.83 kJ/m² | CIPET |
Reading the numbers
A test report is only useful if you know what it says about real windows. Full IS 17953 guide →
Heat reversion
Profiles are heated and measured for shrinkage. Low reversion means frames stay square on hot, west-facing walls and welded corners aren't stressed.
Heat ageing
Samples are held at 150 °C and checked for blisters, cracks or delamination — a sign of good compound and good fusion during extrusion.
Corner strength
Welded L and T corners are loaded in tension and compression until failure. This shows how well the profile and its weld carry real-world loads.
Charpy impact
A notched sample is struck by a pendulum. Higher energy absorption means the profile resists cracking from knocks in transport and installation.
Quality on every shift
- Incoming compound and raw-material checks
- Dimensional checks against drawings at line start-up and during runs
- Surface finish and colour inspection
- Weld-corner trials on production samples
- Counted bundles with printed protective tape
- Lead-free formulation; RoHS-marked packaging
Testing questions
What is CIPET?
CIPET (Central Institute of Petrochemicals Engineering & Technology) is a national institute under the Government of India that tests and certifies plastic products.
What is heat reversion?
It measures how much a profile shrinks after heating. A lower value means the profile holds its dimensions better in heat. IS 17953 sets a maximum of 2.0% for main profiles; Fenplast measured 1.79%.
What does Charpy impact resistance tell me?
It indicates how well the material absorbs a sudden impact without cracking — important during transport, fabrication and installation.
Can I get a copy of the test report?
Yes. Registered fabricators, dealers and project consultants can request the CIPET report from our sales team.
Need the full test report?
Registered fabricators, dealers and consultants can request a copy of our CIPET report.